K403 Nickel-Based Superalloy Spherical High Temperature Alloy Powder
Properties
Product Name: K403 Alloy Powder
Shape: Spherical
Density: ~8.2 g/cm³
Melting Point: ~1300–1350°C
Specifications: Customized processing according to customer needs.
Packaging: Vacuum packaging
Particle size:0-25,15-53,45-105,50-150um Can be supplied according to customer requirements.
Properties: Good high temperature oxidation resistance, heat resistance, corrosion resistance and fatigue resistance.
Usage: Used in aerospace, Marine, petrochemical and energy fields.
Products Usage
1. Thermal Spray Coatings: Used to apply thick coatings resistant to wear, corrosion and oxidation at high temperatures via wire/powder flame or electric arc spraying.
2. Welding: Used as filler material for joining high temperature alloys providing oxidation and corrosion resistance.
3. Brazing: Excellent filler alloy for brazing assemblies operating at over 1000°C like turbine components, heat exchangers etc.
4. Additive Manufacturing: Selective laser melting and other powder bed fusion processes can utilize K403 powder to fabricate parts.
5. Gas Turbines: Powder metallurgy turbine components exposed to hot gas paths like blades, vanes, seals.
6. Chemical Industry: K403 coated components in fluidized bed reactors, heat exchangers, cyclone separators.
7. Glass Industry: Powder sprayed rolls, guides, baffles used in glass melting furnaces and forehearths.
8. Heat Treatment: Fixtures, trays, baskets operating under high temperature applications.
Our normal packaging is 25kgs/Drum
The packaging can be customized. the shipping term can be by sea, by air, and sample or small quantity can be shipped by DHL, FEDEX, EMS and TNT.
Remark: Chemical composition and size can be optimized by the customers' requirements

Conditions for safe storage, including any incompatibilities
Separated from ammonia, strong hydrogen peroxide solutions and strong acids.
Safety Protection
Precautions for safe handling
Handling in a well ventilated place. Wear suitable protective clothing. Avoid contact with skin and eyes. Avoid formation of dust and aerosols. Use non-sparking tools. Prevent fire caused by electrostatic discharge steam.