M247 Nickel-Based Superalloy Spherical High Temperature Alloy Powder

• Trade name: M247

• Origin: Shanghai, China

• Product Type: Alloy powder 

• Size: Customers' Requirements

• Certificate: ISO9001, CE, RoHS, ISO14001

    Properties

    Product Name: M247 Alloy Powder
    Shape: Spherical
    Density: ~8.6 g/cm³
    Melting Point: ~1370–1390°C
    Specifications: Customized processing according to customer needs.
    Packaging: Vacuum packaging
    Particle size: 0-25,15-53,45-105,50-150um Can be supplied according to customer requirements.
    Properties: Good high temperature strength, oxidation resistance, corrosion resistance.
    Usage: Used in aerospace, petrochemical, ship and other fields.

    Products Usage

  • 1. Gas Turbine Blades: Delivers exceptional thermal and mechanical stability.
    2. Combustor Components: Withstands extreme heat and oxidative conditions.
    3. Turbocharger Wheels: Ensures durability under high-speed operations.
    4. Industrial Valves: Resists wear and oxidation in high-temperature environments.

    Packing:
    Our normal packaging is 25kgs/Drum
    The packaging can be customized. the shipping term can be by sea, by air, and sample or small quantity can be shipped by DHL, FEDEX, EMS and TNT.
    Remark: Chemical composition and size can be optimized by the customers' requirements固体1q95固体2gwy
    Conditions for safe storage, including any incompatibilities
    Separated from ammonia, strong hydrogen peroxide solutions and strong acids.

    Safety Protection

    Precautions for safe handling
    Handling in a well ventilated place. Wear suitable protective clothing. Avoid contact with skin and eyes. Avoid formation of dust and aerosols. Use non-sparking tools. Prevent fire caused by electrostatic discharge steam.